Installation and delivery of this spectrometer system is available. This is a 220v Single Phase model and uses high purity Argon gas or Argon + 2% H2 in areas where Argon supply may be an issue.
|
ARL3460
Element
|
Line
|
Iron/Steel base
|
Nickel base
|
Aluminium base
|
Copper base
|
P
|
178.29
|
0.002 - 2
|
0.005 - 2
|
 |
0.0005 - .5
|
S
|
180.73
|
0.002 - 0.3
|
0.01 - 0.4
|
 |
0.0005 - 4
|
B
|
182.64
|
0.0005 - 0.1
|
0.0005 - 0.5
|
 |
 |
C
|
193.09
|
0.005 - 5
|
0.005 - 4
|
 |
0.005 - 2
|
Mo
|
202.03
|
0.005 - 5
|
0.005 - 5
|
 |
 |
Cu
|
224.26
|
0.005 - 10
|
0.1 - 30
|
 |
 |
Co
|
228.62
|
0.001 - 8
|
0.005 - 1
|
 |
0.001 - 0.5
|
Ni
|
231.6
|
0.005 - 3
|
 |
0.005 - 5
|
0.001 - 3
|
Ni
|
243.79
|
3 - 40
|
Int Std
|
 |
 |
Si
|
251.61
|
0.005 - 3
|
0.003 - 3
|
0.001 - 5
|
0.002 - 5
|
Mn
|
263.82
|
0.015 - 20
|
0.0 - 15
|
0.01 - 12
|
0.005 - 10
|
Al
|
266.04
|
 |
 |
Int Std
|
0.0 - 15
|
Cr
|
267.72
|
0.005 - 3
|
0.005 - 3
|
0.001 - 3
|
0.001 - 3
|
Fe
|
273.07
|
Int Std
|
1 - 30
|
 |
0.01 - 10
|
Fe
|
281.33
|
Int Std
|
 |
 |
 |
Mo
|
290.91
|
0.1 - 10
|
0.1 - 30
|
 |
 |
Mn
|
293.31
|
0.005 - 15
|
0.005 - 15
|
0.001 - 2
|
0.005 - 3
|
Cu
|
296.12
|
 |
 |
0.1 - 20
|
Int Std
|
Cr
|
298.92
|
0.5 - 35
|
0.1 - 25
|
 |
 |
V
|
311.07
|
0.001 - 5
|
0.001 - 5
|
0.001 - 5
|
 |
Sn
|
317.51
|
0.01 - 0.5
|
 |
0.001 - 1
|
0.015 - 20
|
Nb
|
319.5
|
0.001 - 4
|
0.005 - 5
|
 |
 |
Ti
|
324.2
|
0.002 - 3
|
0.005 - 5
|
0.001 - 1
|
 |
Cu
|
327.4
|
0 - 0.5
|
0.001 - 0.5
|
0.001 - 0.5
|
 |
Ni
|
331.230
|
1 - 15
|
 |
 |
0.02 - 50
|
Zn
|
334.5
|
0.005 - 0.5
|
 |
0.003 - 10
|
0.001 - 50
|
Fe
|
371.99
|
 |
0.003 - 5
|
0.003 - 2
|
0.002 - 1
|
Mg
|
383.83
|
0.001 - 0.2
|
 |
0.01 - 12
|
 |
Al
|
394.4
|
0.001 - 0.5
|
0.001 - 1
|
 |
0.005 - 1
|
Pb
|
405.78
|
0.001 - 0.5
|
 |
0.002 - 1
|
0.002 - 5
|
|